Material Dimensión (mm) Longitud (mm) Calificación
L 25 x 25 x 4 12000 S235JR/S275JR
L 30 x 30 x 3 12000 S355
L 30 x 30 x 4 12000 S235JR/S275JR
L 30 x 30 x 4 12000 S355
L 35 x 35 x 4 12000 S355
L 35 x 35 x 5 12000 S355
L 40 x 40 x 4 12000 S235JR/S275JR
L 40 x 40 x 4 12000 S355
L 40 x 40 x 5 12000 S235JR/S275JR
L 40 x 40 x 5 12000 S355
L 50 x 50 x 5 12000 S355
L 50 x 50 x 6 12000 S235JR/S275JR
L 50 x 50 x 6 12000 S355
L 60 x 60 x 10 12000 S355
L 60 x 60 x 5 12000 S355
L 60 x 60 x 6 12000 S355
L 60 x 60 x 8 12000 S235JR/S275JR
L 60 x 60 x 8 12000 S355
L 65 x 65 x 5 12000 S355
L 65 x 65 x 6 12000 S355
L 65 x 65 x 7 12000 S355
L 65 x 65 x 8 12000 S355
L 70 x 70 x 10 12000 S355
L 70 x 70 x 6 12000 S355
L 70 x 70 x 7 12000 S355
L 70 x 70 x 8 12000 S235JR/S275JR
L 70 x 70 x 9 12000 S235JR/S275JR
L 75 x 50 x 5 12000 S355
L 75 x 50 x 6 12000 S355
L 75 x 50 x 7 12000 S235JR/S275JR
L 75 x 50 x 7 12000 S355
L 75 x 50 x 8 12000 S355
L 75 x 50 x 9 12000 S355
L 75 x 75 x 10 12000 S355
L 75 x 75 x 6 12000 S235JR/S275JR
L 75 x 75 x 6 12000 S355
L 75 x 75 x 7 12000 S355
L 75 x 75 x 8 12000 S355
L 80 x 40 x 6 12000 S355
L 80 x 80 x 10 12000 S235JR/S275JR
L 80 x 80 x 10 12000 S355
L 80 x 80 x 6 12000 S355
L 80 x 80 x 8 12000 S355
L 90 x 60 x 6 12000 S355
L 90 x 60 x 8 12000 S235JR/S275JR
L 90 x 90 x 10 12000 S355
L 90 x 90 x 11 12000 S355
L 90 x 90 x 12 12000 S355
L 90 x 90 x 13 12000 S355
L 90 x 90 x 8 12000 S355
L 90 x 90 x 9 12000 S355
L 100 x 100 x 10 12000 S355
L 100 x 100 x 11 12000 S355
L 100 x 100 x 12 12000 S355
L 100 x 100 x 16 12000 S355
L 100 x 100 x 8 12000 S355
L 100 x 50 x 10 12000 S235JR/S275JR
L 100 x 50 x 10 12000 S355
L 100 x 50 x 6 12000 S235JR/S275JR
L 100 x 50 x 6 12000 S355
L 100 x 50 x 8 12000 S355
L 100 x 65 x 10 12000 S355
L 100 x 65 x 7 12000 S355
L 100 x 65 x 8 12000 S355
L 100 x 65 x 9 12000 S355
L 100 x 75 x 10 12000 S355
L 100 x 75 x 11 12000 S355
L 100 x 75 x 12 12000 S355
L 100 x 75 x 7 12000 S235JR/S275JR
L 100 x 75 x 7 12000 S355
L 100 x 75 x 8 12000 S355
L 100 x 75 x 9 12000 S355
L 110 x 110 x 10 12000 S355
L 110 x 110 x 12 12000 S355
L 120 x 120 x 10 12000 S355
L 120 x 120 x 12 12000 S235JR/S275JR
L 120 x 120 x 12 12000 S355
L 120 x 120 x 15 12000 S235JR/S275JR
L 120 x 120 x 15 12000 S355
L 120 x 120 x 8 12000 S355
L 120 x 80 x 10 12000 S355
L 120 x 80 x 12 12000 S355
L 120 x 80 x 8 12000 S235JR/S275JR
L 120 x 80 x 8 12000 S355
L 125 x 75 x 10 12000 S355
L 125 x 75 x 12 12000 S355
L 125 x 75 x 8 12000 S355
L 130 x 130 x 10 12000 S355
L 130 x 130 x 12 12000 S355
L 130 x 130 x 14 12000 S235JR/S275JR
L 140 x 140 x 13 12000 S355
L 150 x 100 x 10 12000 S355
L 150 x 100 x 12 12000 S355
L 150 x 100 x 14 12000 S355
L 150 x 100 x 15 12000 S355
L 150 x 150 x 10 12000 S235JR/S275JR
L 150 x 150 x 10 12000 S355
L 150 x 150 x 14 12000 S235JR/S275JR
L 150 x 150 x 14 12000 S355
L 150 x 150 x 15 12000 S355
L 150 x 150 x 16 12000 S235JR/S275JR
L 150 x 150 x 16 12000 S355
L 150 x 150 x 18 12000 S355
L 150 x 150 x 20 12000 S235JR/S275JR
L 150 x 150 x 20 12000 S355
L 150 x 75 x 10 12000 S355
L 150 x 75 x 11 12000 S355
L 150 x 75 x 12 12000 S355
L 150 x 75 x 15 12000 S235JR/S275JR
L 150 x 75 x 15 12000 S355
L 150 x 75 x 9 12000 S355
L 150 x 90 x 10 12000 S355
L 150 x 90 x 12 12000 S355
L 150 x 90 x 15 12000 S235JR/S275JR
L 150 x 90 x 15 12000 S355
L 160 x 160 x 15 12000 S235JR/S275JR
L 160 x 160 x 15 12000 S355
L 160 x 160 x 17 12000 S235JR/S275JR
L 160 x 160 x 17 12000 S355
L 160 x 80 x 10 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S355
L 180 x 180 x 18 12000 S235JR/S275JR
L 180 x 180 x 18 12000 S355
L 180 x 180 x 20 12000 S235JR/S275JR
L 180 x 180 x 20 12000 S355
L 180 x 180 x 22 12000 S355
L 180 x 90 x 10 12000 S355
L 200 x 100 x 10 12000 S235JR/S275JR
L 200 x 100 x 10 12000 S355
L 200 x 100 x 12 12000 S235JR/S275JR
L 200 x 100 x 12 12000 S355
L 200 x 100 x 14 12000 S235JR/S275JR
L 200 x 100 x 14 12000 S355
L 200 x 100 x 15 12000 S235JR/S275JR
L 200 x 100 x 15 12000 S355
L 200 x 100 x 16 12000 S235JR/S275JR
L 200 x 100 x 16 12000 S355
L 200 x 150 x 12 12000 S235JR/S275JR
L 200 x 150 x 12 12000 S355
L 200 x 150 x 15 12000 S235JR/S275JR
L 200 x 150 x 15 12000 S355
L 200 x 200 x 16 12000 S235JR/S275JR
L 200 x 200 x 16 12000 S355
L 200 x 200 x 18 12000 S235JR/S275JR
L 200 x 200 x 18 12000 S355
L 200 x 200 x 20 12000 S235JR/S275JR
L 200 x 200 x 20 12000 S355
L 200 x 200 x 22 12000 S235JR/S275JR
L 200 x 200 x 22 12000 S355
L 200 x 200 x 24 12000 S235JR/S275JR
L 200 x 200 x 24 12000 S355
L 200 x 200 x 26 12000 S235JR/S275JR
L 200 x 200 x 26 12000 S355
L 200 x 200 x 28 12000 S235JR/S275JR
L 200 x 200 x 28 12000 S355
L 200 x 200 x 34 12000 S355
L 250 x 250 x 18 12000 S235JR/S275JR
L 250 x 250 x 18 12000 S355
L 250 x 250 x 20 12000 S235JR/S275JR
L 250 x 250 x 20 12000 S355
L 250 x 250 x 22 12000 S235JR/S275JR
L 250 x 250 x 22 12000 S355
L 250 x 250 x 24 12000 S235JR/S275JR
L 250 x 250 x 24 12000 S355
L 250 x 250 x 25 12000 S355
L 250 x 250 x 26 12000 S235JR/S275JR
L 250 x 250 x 26 12000 S355
L 250 x 250 x 28 12000 S355
L 250 x 250 x 30 12000 S355
L 250 x 250 x 35 12000 S355
L 250 x 90 x 10 12000 S235JR/S275JR
L 250 x 90 x 10 12000 S355
L 250 x 90 x 12 12000 S235JR/S275JR
L 250 x 90 x 12 12000 S355
L 250 x 90 x 14 12000 S235JR/S275JR
L 250 x 90 x 14 12000 S355
L 250 x 90 x 16 12000 S235JR/S275JR
L 250 x 90 x 16 12000 S355
PRS Hea 100 12000 S235JR/S275JR
PRS Hea 100 12000 S355
PRS Hea 120 12000 S235JR/S275JR
PRS Hea 120 12000 S355
PRS Hea 140 12000 S235JR/S275JR
PRS Hea 140 12000 S355
PRS Hea 160 12000 S235JR/S275JR
PRS Hea 160 12000 S355
PRS Hea 180 12000 S235JR/S275JR
PRS Hea 180 12000 S355
PRS Hea 200 12000 S235JR/S275JR
PRS Hea 200 12000 S355
PRS Hea 220 12000 S355
PRS Hea 260 12000 S355
PRS Hea 300 12000 S355
PRS HEB 100 12000 S235JR/S275JR
PRS HEB 100 12000 S355
PRS Heb 120 12000 S235JR/S275JR
PRS Heb 120 12000 S355
PRS Heb 140 12000 S235JR/S275JR
PRS Heb 140 12000 S355
PRS Heb 160 12000 S235JR/S275JR
PRS Heb 160 12000 S355
PRS Heb 180 12000 S235JR/S275JR
PRS Heb 200 12000 S235JR/S275JR
PRS Heb 200 12000 S355
PRS IPE 100 12000 S235JR/S275JR
PRS IPE 120 12000 S235JR/S275JR
PRS IPE 140 12000 S235JR/S275JR
PRS IPE 160 12000 S235JR/S275JR
PRS IPE 160 12000 S235JR/S275JR
PRS IPE 220 12000 S355
PRS IPE 240 12000 S355
PRS IPE 270 12000 S355
PRS IPE 300 12000 S355
PRS IPE 550 12000 S355
PRS IPE 80 12000 S235JR/S275JR
PRS IPN 360 12000 S235JR/S275JR
PRS IPN 80 12000 S235JR/S275JR
PRS UPE 80 12000 S355
PRS UPE 100 12000 S355
PRS UPE 120 12000 S355
PRS UPE 140 12000 S355
PRS UPE 160 12000 S355
PRS UPE 180 12000 S355
PRS UPE 200 12000 S235JR/S275JR
PRS UPE 200 12000 S355
PRS UPE 220 12000 S355
PRS UPE 240 12000 S355
PRS UPE 300 12000 S355
PRS UPE 400 12000 S355

Tenemos más de 10000 m² de espacio de almacenamiento y mantenemos relaciones cercanas con cientos de proveedores y molinos de acero en Europa y en todo el mundo. Esto nos permite entregar rápidamente cualquier tamaño o calificación que no esté disponible en nuestras acciones a los mejores precios y plazos de entrega.

Nuestro stock incluye principalmente:

• Productos de acero estructural (IPE, UPE, UPN, HEA, HEB, ángulos iguales y desiguales) en los grados S235JR, S275JR, S355J2

• Hojas y bobinas de acero en caliente (3 mm a 12 mm, DD11/S235JR+N/S355MC, en escabeche y engrasado)

• Hojas y bobinas de acero galvanizado (0. 5 mm a 4 mm, dx 51+ z)

• Hojas y bobinas de acero enrollado en frío (DC01)

• Bars T, barras planas, barras redondas, barras cuadradas y secciones huecas (EN 10219 o EN 10210)

• Productos de acero inoxidable (barras, sábanas, placas)

• Placas pesadas (6 mm a 300 mm en cualquier tamaño y grado)