La placa de acero ASTM A515 es una especificación para placas de recipientes a presión diseñadas para su uso en aplicaciones de temperatura moderada a alta-. Este material se utiliza principalmente en la fabricación de recipientes a presión y calderas industriales, donde son esenciales una alta resistencia y una excelente tenacidad. Incluye tres grados: ASTM A515 Grado 60, Grado 65 y Grado 70.
Estándar: ASTM A515/A515M
Grado de acero: A515 GR 60 (415), A515 GR 65 (450), A515 GR 70 (485)
Espesor: 3 mm -500 mm
Ancho: 1000 mm-4000 mm
Longitud: 1000 mm-18000 mm
Requisitos de composición química
| Placas para recipientes a presión ASTM A515 | ||||
|---|---|---|---|---|
| Elemento | Gr. 60 | Gr. 65 | Gr. 70 | |
| C máximo |
t Menor o igual a 1" | 0.24 | 0.28 | 0.31 |
| 1"< t ≤2" | 0.27 | 0.31 | 0.33 | |
| 2"< t ≤4" | 0.29 | 0.33 | 0.35 | |
| 4"< t ≤8" | 0.31 | 0.33 | 0.35 | |
| t>8" | 0.31 | 0.33 | 0.35 | |
| Minnesota máximo |
*H.A. | 0.90 | 0.90 | 1.20 |
| *P.A. | 0.98 | 0.98 | 1.30 | |
| P | máximo | 0.025 | 0.025 | 0.025 |
| S | máximo | 0.025 | 0.025 | 0.025 |
| Si | *H.A. | 0.15–0.40 | 0.15–0.40 | 0.15–0.40 |
| *P.A. | 0.13–0.45 | 0.13–0.45 | 0.13–0.45 | |
Requisitos de tracción
| ASTM A515 | *T.S. MPa [ksi] |
*Y.S. MPa [ksi] |
*EL. 8" mín. % |
*EL. 2" mín. % |
|---|---|---|---|---|
| Grado 60 | 415–550 [60–80] |
Mayor o igual a 220 [Mayor o igual a 32] |
21 | 25 |
| Grado 65 | 450–585 [65–85] |
Mayor o igual a 240 [Mayor o igual a 35] |
19 | 23 |
| Grado 70 | 485–620 [70–90] |
Mayor o igual a 260 [Mayor o igual a 38] |
17 | 21 |
Aplicaciones

Las placas de acero ASTM A515 se utilizan comúnmente en:
- Fabricación de recipientes a presión para la industria del petróleo y el gas.
- Construcción de calderas e intercambiadores de calor.
- Fabricación de tanques de almacenamiento industriales y otros equipos-sensibles a la presión.
- Aplicaciones donde se requiere alta resistencia y durabilidad, especialmente en entornos de alta-temperatura.
- En resumen, las placas de acero ASTM A515 brindan una solución robusta y confiable para diversas aplicaciones en los sectores de fabricación de calderas y recipientes a presión, garantizando seguridad y rendimiento en condiciones exigentes.
Si desea conocer más sobre los productos de GNEE, puede enviar un correo electrónico aalloy@gneesteelgroup.com.Estamos más que felices de poder ayudarle.
| Grados de placas para recipientes a presión suministradas por GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grado A | ASTM A202 Grado B | ||
| ASTM A203/A203M | ASTM A203 Grado A | ASTM A203 Grado B | ASTM A203 Grado D | ASTM A203 Grado E | |
| ASTM A203 Grado F | |||||
| ASTM A204/A204M | ASTM A204 Grado A | ASTM A204 Grado B | ASTM A204 Grado C | ||
| ASTM A285/A285M | ASTM A285 Grado A | ASTM A285 Grado B | ASTM A285 Grado C | ||
| ASTM A299/A299M | ASTM A299 Grado A | ASTM A299 Grado B | |||
| ASTM A302/A302M | ASTM A302 Grado A | ASTM A302 Grado B | ASTM A302 Grado C | ASTM A302 Grado D | |
| ASTM A387/A387M | ASTM A387 Grado 5 Clase1 | ASTM A387 Grado 5 Clase 2 | ASTM A387 Grado 11 Clase 1 | ASTM A387 Grado 11 Clase 2 | |
| ASTM A387 Grado 12 Clase1 | ASTM A387 Grado 12 Clase 2 | ASTM A387 Grado 22 Clase 1 | ASTM A387 Grado 22 Clase 2 | ||
| ASTM A515/A515M | ASTM A515 Grado 60 | ASTM A515 Grado 65 | ASTM A515 Grado 70 | ||
| ASTM A516/A516M | ASTM A516 Grado 55 | ASTM A516 Grado 60 | ASTM A516 Grado 65 | ASTM A516 Grado 70 | |
| ASTM A517/A517M | ASTM A517 Grado A | ASTM A517 Grado B | ASTM A517 Grado E | ASTM A517 Grado F | |
| ASTM A517 Grado P | ASTM A517 Grado J | ||||
| ASTM A533/A533M | ASTM A533 Grado A Clase1 | ASTM A533 Grado B Clase 1 | ASTM A533 Grado C Clase 1 | ASTM A533 Grado D Clase 1 | |
| ASTM A533 Grado A Clase 2 | ASTM A533 Grado B Clase 2 | ASTM A533 Grado C Clase 2 | ASTM A533 Grado D Clase 2 | ||
| ASTM A533 Grado A Clase 3 | ASTM A533 Grado B Clase 3 | ASTM A533 Grado C Clase 3 | ASTM A533 Grado D Clase 3 | ||
| ASTM A537/A537M | ASTM A537 Clase 1 | ASTM A537 Clase 2 | ASTM A537 Clase 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grado A | ASTM A662 Grado B | ASTM A662 Grado C | ||
| ES | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| ES10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JISG3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| ES | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| ESTRUENDO | DIN 17155 | DIN 17155 ALTA | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||