GB713 13MnNiMoR Pressure Vessel Steel Plate

GB713 13MnNiMoR Pressure Vessel Steel Plate

13MnNiMoR is a low-alloy high-strength quenched and tempered steel plate for pressure vessels, conforming to the standard GB 19189-2011. It is mainly used to manufacture large pressure vessels, boilers, storage tanks and other pressure-bearing equipment, and is especially suitable for working conditions with low temperature, high pressure and corrosive media.
Envíeconsulta
Chatee ahora
Descripción
Parámetros técnicos

GB 713 alloy pressure vessel steel 13MnNiMoR.13MnNiMoR boiler plate shall be done low temperature impacting test under 0 centigrade.We stock many sizes of these boiler steel plates at port warehouses which are ready for shipment,contact us for stock details.

 

GB713 13MnNiMoR Pressure Vessel And Boiler Steel Plate Chemical Composition and Mechanical Property

C% V% P% S%
13MnNiMoR <=O.15 0.15-0.50 1.20-1.650 0.20-0.40 0.60-1.0 0.20-0.40 0.005-0.020 <=0.020 <=0.010  
13MnNiMoR 30<> 570-720 390 18
100<> 380

 



Mean coefficient of thermal expansion 10-6/(℃) between 20(℃) and



31 - -     0.12 -  
858 447 - 44.3 341   -  
767 - 31 43.2     323 213

 

GB713 13MnNiMoR Pressure Vessel Steel

GB713 13MnNiMoR Pressure Vessel Steel

A:We are a professional manufacture and have many years production and management experience.

A:We accept FOB,CIF,CFR and other international shipping terms.Port of loading can be specified according to customer requirements.

Etiqueta: gb713 13mnnimor pressure vessel steel plate, China gb713 13mnnimor pressure vessel steel plate manufacturers, suppliers, factory, 12CR1MOVR Placa de acero del recipiente, 14cr1mor material de placa de recipiente a presión, 14cr1Mor de acero de calidad del recipiente a presión, Acero de recipiente a presión GB, Q345R Hoja de recipientes a presión, Q345R Placa de acero de recipiente a presión